Cracks, delaminations, and defective joints are often invisible from the outside. Active thermography reveals these hidden material defects by analyzing how they affect heat distribution within a component. But which thermographic testing method is best suited to which application? We explore six important methods, explain how they work, and highlight where their individual strengths lie.
Every object emits infrared radiation, which can be captured by an infrared camera and visualized as a thermal image. In non-destructive testing (NDT), this principle is used to analyze temperature distributions and assess the condition of components.
Two main approaches can be distinguished:
Passive thermography uses temperature differences that already exist, for example those caused by friction, electrical losses, or heat generated during operation. This makes it possible to identify thermal anomalies and analyze the functional behavior of components.
Active thermography takes this a step further: Energy is deliberately introduced into the test object to generate a thermal response. Cracks, air inclusions, delaminations, and other material irregularities influence how heat is generated or propagates through the material. The resulting temperature patterns are recorded by an infrared camera and analyzed using suitable evaluation methods.
This makes it possible to detect defects that would remain hidden during conventional visual inspection.
A thermal image does not directly show the inside of a component. Instead, it reveals how material defects influence the thermal response measured at the surface.
For example, a crack can interrupt heat flow or change the distribution of induced electrical currents, resulting in localized temperature differences. Delaminations and air inclusions, on the other hand, can act as thermal barriers, slowing down heat transfer between material layers.
Depending on the excitation method, defects may appear as localized hot or cold spots or become visible through differences in heating and cooling behavior.
Advanced image processing techniques, including phase and amplitude analysis, help distinguish these defect-related signals from the surrounding material. This allows even subtle thermal anomalies to be detected and evaluated.
Not all materials respond to thermal excitation in the same way. While eddy currents are particularly effective for heating electrically conductive materials, optical and mechanical excitation methods can also be used for plastics, ceramics, and fiber-reinforced composites.
The main differences lie in how energy is introduced and how the excitation is controlled over time.
Some methods can also be combined. For example, induction or laser-based testing can use pulsed or periodically modulated excitation, while scanning describes how an excitation source moves across the component. The following six methods therefore represent complementary approaches rather than entirely separate technologies.
Induction thermography uses an alternating electromagnetic field to introduce energy into electrically conductive materials without physical contact. The field generates eddy currents within the component, causing the material to heat up. The distribution of these currents depends on the material properties, component geometry, and the presence of defects.
Cracks and other irregularities disturb the current flow, creating localized changes in current density and heat generation. These effects produce characteristic temperature patterns, which are captured by a high-resolution infrared camera. Surface-breaking cracks, in particular, can generate strong thermal contrasts, making even small defects visible.
Depending on the inspection requirements, inductive excitation can be applied in short pulses or periodically modulated for lock-in evaluation. The excitation frequency, inductor geometry, and measurement parameters can be adapted to the component and expected defect characteristics. This flexibility enables targeted inspection of complex surfaces, edges, and other challenging areas.
Key advantage: Fast, contactless crack detection with adaptable electromagnetic excitation makes induction thermography particularly suitable for automated quality control and series production.
Typical applications: Crack detection in forged and cast components, gears, shafts, metallic long products, and welds.
Lock-in thermography uses periodically modulated thermal excitation to generate controlled temperature oscillations within a component. The heat is typically introduced using halogen lamps or infrared emitters, while an infrared camera records the thermal response in synchronization with the excitation.
As heat propagates through the material, defects such as delaminations, air inclusions, or insufficient bonding alter the local thermal behavior. These changes affect both the amplitude and timing of the temperature response. By analyzing the recorded image sequences, the system generates amplitude and phase images that highlight differences between intact and defective material regions.
Phase analysis is particularly valuable because it can reduce the influence of uneven heating, surface emissivity variations, and other interfering factors. This makes subtle thermal anomalies easier to identify than in conventional temperature images.
Another important feature is the relationship between excitation frequency and thermal penetration depth. Lower modulation frequencies generally allow the thermal response to probe deeper material regions, while higher frequencies emphasize areas closer to the surface.
Key advantage: Sensitive, phase-based evaluation improves defect contrast and supports reproducible inspection of hidden irregularities in multilayer structures, even under challenging surface conditions.
Typical applications: Delaminations in fiber-reinforced composites, air inclusions, adhesive bonding defects, coating and wall thickness variations, and hidden irregularities in multilayer materials.
Pulse thermography typically uses an intense, short energy pulse generated by high-power flash lamps to heat the surface of a component. The excitation produces a rapid temperature increase, followed by a cooling phase that is continuously recorded by an infrared camera.
As heat diffuses into the material, subsurface defects influence the way thermal energy is transported. Delaminations, pores, and bonding defects can interrupt heat flow, causing affected regions to cool differently from the surrounding material. These differences become visible as characteristic temperature contrasts over time.
Rather than evaluating a single thermal image, pulse thermography analyzes a sequence of images captured during the cooling process. Depending on the inspection task, the data can be processed using temperature contrast analysis, temporal signal reconstruction, or phase-based evaluation. These methods improve defect visibility and provide additional information about the thermal behavior of the material.
Because a single energy pulse can cover a relatively large inspection area, the method is particularly attractive for examining flat components, coatings, and composite structures.
Key advantage: Short excitation times and large-area image acquisition enable efficient inspection, particularly when high throughput and the detection of near-surface defects are required.
Typical applications: Near-surface delaminations, porosity, coating defects, adhesive bonding failures, and hidden irregularities in fiber-reinforced composites and sandwich structures.
Laser thermography uses focused laser radiation to introduce thermal energy into a precisely defined area of a component. Unlike large-area optical excitation, the laser allows heat to be applied selectively to individual points, lines, or critical inspection regions.
The localized heating generates a thermal response that propagates through the surrounding material. Cracks, pores, delaminations, and other inhomogeneities influence this heat flow, creating characteristic temperature patterns that can be detected and analyzed using an infrared camera.
The laser intensity, excitation duration, and beam geometry can be adapted to the material and inspection task. Depending on the application, energy can be introduced as a short pulse, through periodic modulation, or over a defined heating period. These excitation strategies provide flexibility when investigating different defect types and material properties.
Precisely controlled energy input is particularly beneficial for complex geometries, narrow inspection zones, and applications where heating the entire component would be unnecessary or impractical.
Key advantage: Highly localized, flexible energy input enables targeted inspection of small areas and challenging geometries that may be difficult to examine using conventional large-area heating methods.
Typical applications: Crack detection in welds and joints, grinding burn inspection, evaluation of hardened zones, coating defects, and material irregularities in metallic and non-metallic components.
Key advantage: Highly localized, flexible energy input enables targeted inspection of small areas and challenging geometries that may be difficult to examine using conventional large-area heating methods.
Typical applications: Crack detection in welds and joints, grinding burn inspection, evaluation of hardened zones, coating defects, and material irregularities in metallic and non-metallic components.
Scanning laser thermography, also known as flying-spot thermography, builds on the principle of laser-based thermal excitation. Instead of heating a stationary area, a focused laser beam is moved across the component surface along a defined scanning path.
As the laser travels over the surface, it generates a localized temperature field that follows the excitation point. Heat spreads from the heated area into the surrounding material, while cracks and other inhomogeneities disturb this propagation. The resulting thermal signatures are recorded by an infrared camera and evaluated to identify potential defects.
The movement of the laser provides additional flexibility in how the inspection is performed. Depending on the component geometry, the beam can scan larger surfaces, follow weld seams, or concentrate on critical features such as edges, transitions, and internal radii.
By combining controlled laser movement with synchronized thermal imaging, the method allows detailed examination of geometrically challenging components. Scan paths and measurement parameters can be adapted to individual inspection requirements, supporting both laboratory investigations and automated industrial applications.
Key advantage: High spatial resolution and flexible scanning strategies enable precise inspection of narrow structures, complex contours, and critical surface regions.
Typical applications: Surface and near-surface cracks in welds, edges, and bores, inspection of complex three-dimensional components, and defect detection in ceramics, plastics, sintered materials, and metallic structures.
Ultrasound-excited thermography uses mechanical vibration rather than external thermal radiation to generate a measurable temperature response. High-frequency ultrasonic energy is introduced into the component, typically through a mechanically coupled sonotrode, causing the material to vibrate.
At locations such as cracks, poorly bonded interfaces, or delaminations, the mechanical response differs from that of intact material. Friction between contacting defect surfaces, internal damping, and other energy dissipation mechanisms can convert part of the vibrational energy into localized heat. An infrared camera captures these temperature changes and visualizes the corresponding defect indications.
Unlike methods that primarily rely on heat propagating from an externally heated surface, ultrasound-excited thermography can generate thermal signals directly at defects that respond to mechanical excitation. This can provide high defect contrast, particularly for fatigue cracks and defective material interfaces.
The ultrasonic energy can be introduced in short bursts or using periodically modulated excitation. Depending on the approach, the recorded signals can be analyzed through temperature differences or phase and amplitude evaluation. Reliable results require suitable excitation parameters and reproducible mechanical coupling to the component.
Key advantage: Defect-selective heat generation allows cracks and bonding defects that respond to mechanical vibration to be identified with high thermal contrast, while infrared image acquisition remains contactless.
Typical applications: Microcracks and fatigue cracks, delaminations in fiber-reinforced composites, adhesive bonding defects, and flaws in welded or spot-welded joints.
Each method offers specific advantages depending on the material and inspection requirements. The following comparison highlights their main characteristics and typical applications.
Choosing the right thermographic testing method requires more than matching a technology to a material. Defect characteristics, component geometry, inspection depth, and production requirements all influence the decision.
Two practical examples illustrate how these factors help determine the most suitable inspection approach.
Consider a forged gear or a geometrically complex metal component that may develop fine surface cracks during manufacturing. These defects can be difficult to identify through visual inspection, particularly around edges, transitions, or other challenging geometries.
Induction thermography provides a suitable approach because induced eddy currents interact directly with the electrically conductive material. Surface-breaking cracks disturb the current distribution and can create localized thermal signatures.
The contactless excitation and short inspection times make the method particularly attractive for repetitive quality checks and integration into automated production environments.
Want to learn more? Our article on induction thermography for component testing takes a closer look at the testing principle, characteristic crack patterns, and automated inspection of complex surfaces.
Fiber-reinforced composites are widely used in lightweight structures where high strength and low weight are essential. However, internal delaminations or defective bonds may compromise structural integrity without producing visible surface damage.
Optical active thermography offers different approaches for examining these materials. Pulse thermography is particularly suitable for quickly inspecting larger surfaces for near-surface defects. Lock-in thermography uses periodically modulated excitation to analyze thermal responses at different depths, making it valuable for more detailed investigations of layered structures.
The choice depends on the expected defect depth, material properties, and required inspection speed. In some cases, combining different excitation and evaluation approaches can provide additional information.
Although active thermography offers considerable flexibility, not every defect can be detected equally well. The quality of the inspection depends on several interacting factors.
Material properties: Thermal conductivity and diffusivity influence how quickly heat spreads through a component. Electrical conductivity also determines whether inductive excitation is suitable.
Surface conditions: Surface emissivity, reflections, coatings, and variations in surface finish can affect infrared measurements. Suitable excitation and evaluation methods help reduce these influences.
Defect geometry and depth: The size, orientation, and location of a defect determine how strongly it influences the thermal response. Deeper or very small defects may produce weaker signals that are more difficult to distinguish.
Inspection parameters: Excitation intensity, measurement duration, camera resolution, and evaluation algorithms all affect the achievable defect contrast and inspection reliability.
For these reasons, selecting a thermography method requires more than choosing an excitation source. The entire inspection process must be adapted to the component and the defects that need to be detected.
Application-specific feasibility studies using representative test parts help establish suitable inspection parameters and determine whether the required detection performance can be achieved under realistic conditions.
From research and development to automated series inspection, active thermography provides versatile solutions for non-destructive evaluation. Modern infrared cameras, controlled excitation systems, and advanced evaluation software enable reproducible inspections, digital documentation, and integration into industrial production processes.
With edevis as part of the FOERSTER Group, extensive experience in industrial non-destructive testing is combined with specialized expertise in active thermography. Together, we offer a broad range of technologies for different materials, components, and inspection requirements – from initial feasibility studies to automated industrial inspection solutions.
Discover the possibilities of active thermography! Explore our edevis thermography portfolio and find the right solution for your inspection needs.
Want to see our technology in action? Book a demo with our experts and discover how thermography can support your specific testing application.